Corrosion Analysis of Shell and Tube Heat Exchanger

Dec 08, 2021

In the manufacture of shell-and-tube heat exchangers, manual arc welding is generally used for the welding of tube sheets and tubes. The weld shape has defects of varying degrees, such as depressions, pores, slag inclusions, etc., and the weld stress distribution is not uniform. When in use, the tube sheet is generally in contact with industrial cooling water, and impurities, salts, gases, and microorganisms in the industrial cooling water will cause corrosion to the tube sheet and welds. This is what we often call electrochemical corrosion. Studies have shown that industrial water, whether it is fresh water or sea water, will have various ions and dissolved oxygen, among which the concentration of chloride ions and oxygen changes, which play an important role in the corrosive shape of metals. In addition, the complexity of the metal structure will also affect the corrosion morphology. Therefore, pitting corrosion and crevice corrosion are the main corrosion of the welded seam of tube sheet and tube. From the outside, there will be many corrosion products and sediments on the surface of the tube sheet, and pits of different sizes are distributed. When seawater is used as the medium, galvanic corrosion will also occur. Chemical corrosion is the corrosion of the medium, and the tube sheet of the heat exchanger will be corroded by the chemical medium when it comes in contact with a variety of chemical media. In addition, a certain amount of bimetallic corrosion occurs between the heat exchanger tube sheet and the heat exchange tube.


Znajomość branży